Weld
seam quality is a key factor.
If the welding criteria along the flow paths in the weld chamber are
not satisfied,
weld
seam defects may appear in the profile. Welding criteria are
expressed in terms of pressure, temperature and flow within the weld chamber.
The
MTD
3D flow solver permits to predict those quantities in terms of die
geometry and process parameters.
In the example below, the flow through
the large press die below was simulated for different die conceptions, until
satisfaction of the weld criterion, thus leading to satisfactory profile
quality.